The second volume of the topic series “Superalloys” contains articles published by Trans Tech Publications from 2018 up to 2019. This collection presents a wide range of scientific research results and engineering solutions in the field of alloy developments and performance, physical and mechanical properties, and processing technologies of various types of superalloys. We hope this collection will be beneficial and interesting to a broad audience of researchers and engineers from the area of materials science and engineering.
Les mer
Aggregated Book
- Preface
- Chapter 1: Physical and Mechanical Metallurgy of Ni-Based Superalloys
- Effects of Solid Solution Temperature on Microstructure and Properties of Extruded and Forged FGH95 Superalloys
- Microstructure-Dependent Deform Behavior of a Polycrystalline Ni-Based Superalloy Based on Micropillar Compression
- Heat Treatments Effects on NickeI-Based Superalloy Inconel 713C
- Investigation on Microvoid Nucleation of High Temperature Nickel Based Superalloy under Thermal Shock
- Effects of Original Microstructure on Hot Deformation Behavior and Microstructure of a P/M Ni-Base Superalloy
- Comparison of Semisolid Microstructure Evolution of Wrought Nickel Based Superalloy GH4037 with Different Solid Fraction
- Low Cycle Fatigue Life Evaluation According to Temperature and Orientation in Nickel-Base Superalloy
- Low-Temperature Superplasticity of the Ni-Based EK61 Superalloy and Application of this Effect to Obtain Solid Phase Joints
- Observations on Dynamic Strain Aging Manifestation in Inconel 718 Superalloy
- Service Temperature Evaluation of Cast K465 Superalloy Turbine Vane Based on Microstructural Evolution
- Microstructure Evolution of Nickel-Based Superalloys Induced by Thermomechanical Processing - Simulation and Verification
- Study of Mechanical Degradation and Microstructural Characterization in a Ni-Based Superalloy Component of a Gas Turbine
- Deformation Twinning Behavior in High Ni-Austenitic Materials
- Hot Corrosion of Alloy 617 OCC in Simulated USC Power Plant Environment
- Segregation and Precipitation Behavior of Phosphorus in a Ni-Fe-Cr Base Wrought Superalloy
- Chapter 2: Single-Crystal and Directionally Solidified Superalloys
- Creep Properties and Microstructural Evolution at 760°C/785MPa of a Re-Containing Single Crystal Superalloy
- Deformation Features of a High Mo Nickel-Based Single Crystal Superalloy during Creep at High Temperature
- Creep Damage of a Re/Ru-Containing Single Crystal Nickel-Based Superalloy at Elevated Temperature
- Features of the Formation of Structure and Phases in Single-Crystal High-Temperature Alloys and their Effect on Mechanical Properties
- Thermodynamic Study on Equilibrium Phases in Nickel-Base Single Crystal Superalloys
- Formation of Secondary Phases in the Boundary between Surface Defect Grains and Matrix in Third Generation Nickel-Based Single Crystal Superalloy Turbine Blades
- The DSC Investigation on Phase Transformations of Directionally Solidified (DS) and Powder Metallurgy (PM) Ni-Base Superalloys
- Chapter 3: Polycrystalline Low Nickel Superalloys
- Thoughts on High Performance Superalloy Design and Microstructural Characteristics of a Newly Designed Ni-Cr-Co-W Superalloy Applied above 850°C
- Influence of Water Vapor on Oxide Scale Morphology of Incoloy800HT at 850°C
- Study on Heat Treatment of a Low Nickel Superalloy Used for Automotive Valves
- Corrosion Behavior of Incoloy 825 in High Temperature Vapor Containing Sodium Chloride
- An Improved Omega-Based Method for Creep Life Prediction Using Hyperbolic Sine Stress Correlation
- Creep Damage Mechanisms in Cast Cobalt Superalloys for Applications in Glass Industry
- Impact of L12-Ordered Precipitation on the Strength of Alumina-Forming Austenitic Heat-Resistant Steels
- Chapter 4: Superalloys Processing and Manufacturing
- Optimization of Spot Welding Parameters in Similar and Dissimilar Alloys AISI-321 and Inconel-X750 Alloys
- Effect of Hot Extrusion on the Flow Behaviour of a Nickel-Based P/M Superalloy
- Effects of Preheating Temperature at Primary Shear Zone in Laser Assisted Milling Process
- Evaluation of Surface Roughness and Tool Wear in High Speed Machining of Inconel 718
- The Enhanced Ability to Withstand Axial Hot Compression of Electropulsing-Assisted Ultrasonic Surface Rolling Process Treated Inconel 718
- Experimental Study of Cutting Performance for Inconel 718 Milling by Various Assisted Machining Techniques
- Fabrication and EDM Corrosion Resistance of Copper Electroforming Layer on Tube Electrode for Aero-Engine Blade Cooling Hole in EDM Process
- The Influence of Laser Drilling Process on the Microstructural Changes of Nickel Based Superalloy
- Microstructure Characterization of Superalloy 718 during Dissimilar Rotary Friction Welding
- Microstructure Characterization in Dissimilar TIG Welds of Inconel Alloy 718 and High Strength Tensile Steel
- Mechanical Properties and Fatigue Resistance of 3D Printed Inconel 718 in Comparison with Conventional Manufacture
- Failure Analysis of Hot Clamp Induced Cracking on Hydrogen Reformer Outlet Pigtail Tubes
- Solution Treatment Process of Haynes 230 Cylindrical Blank Used for Hot Flow Spinning
- Research of Effect of the Powder Material Quality in the Structure Formation of the DLD Inconel 718 Samples
- Analysis of Dimensional Accuracy (Over Cut) and Surface Quality (Roughness) in Electrical Discharge Machining of Inconel-718 Alloy
- Optimization of Process Parameters in the Turning Operation of Inconel 625
- Investigation of the Impact of Cutting Parameters on Surface Integrity in the End Milling of Inconel 625
- The Study of Deformability of Heat-Resistant Alloy Named “Inconel Alloy 625” for Estimation of Plates Production Possibility at Wide-Strip Rolling “Mill 2300”
- Yb: YAG Laser Welding of Aeronautical Alloys
- Laser Beam Welding of IN792 DS Superalloy
- Selective Laser Melting of Inconel 718 under High Power and High Scanning Speed Conditions
- Compositional Optimization of In718 Superalloy Powder for Additive Manufacturing
- Chapter 5: Coatings for Superalloys
- Investigation of Hot Section (Nozzle Guiding Vane) Distress due to Interaction of Thermal Barrier Coatings with CMAS
- Microstructural Change and Fracture Behavior under Different Heat Exposure Conditions on Thermal Barrier Coatings Deposited on TiAl Intermetallic Compound
- Development of Evaluation Method for Damage of Oxidation CoNiCrAlY Coating
- Experimental Study of High Velocity Oxygen Fuel Sprayed Cr3C2- Ni-Cr-B-Si Coatings on Inconel 718 Using Design of Experiments
- Features of Creating Nanostructured Intermetallic Ti-Al-Si-Cr Coatings for the Hot Section Part of Gas Turbine Engines
- Microstructure and Positron Lifetimes of Aluminide Coatings on Inconel 713
- Degradation of HVOF Sprayed Hastelloy C-276 Local Mechanical Properties after Exposure to High Temperature Corrosion
- Evaluation of Microstructure, Phase Composition and Hardness of Alternative Abradable Ceramic Coating Systems Produced by Means of Atmospheric Plasma Spraying
- Hydrogen Influence on Microstructure and Properties of Novel Explosive Welded Corrosion Resistant Clad Materials
- Laser Surface Treatment of Sintered Stainless Steels for Wear Resistance Enhancement
- Thermo-Physical Properties Measurement of Advanced TBC Materials with Pyrochlore and Perovskite Structures
- Microstructure and Abrasive Wear Behaviour of Nickel Based Hardfacing Stainless Steel Deposited by Gas Metal Arc Welding
- Study of Wear on Nicraly Coating Sprayed by HVOF on 316 Steel and Laser CO2 Remelting Process
- Preparation of Dense Al2O3 Film on 8YSZ Coating by Sol-Gel Method
- The Impedance Spectroscopy Study of the Oxides Layer in Thermal Barrier Coatings
- Influence of Zirconia Powder Fractional Composition on Microstructure and Properties of Thermal Barrier Coating Obtained by Thermal Spraying
- Chapter 6: Superalloys Deformation and Property Computational Modelling
- Comprehensive Numerical Simulation of Stress and Damage Fields under Thermo-Mechanical Loading for TBC-Coated Ni-Based Superalloy
- Thermal Deformation Behavior and Formability of High Temperature with Corrosion Resistance Alloy
- Comparison of Different FEM Software in Terms of Hot Ultrasonic Assisted Machining Technique
- Establishment of the High Temperature Constitutive Relationship of the Haynes 230 Ni-Based Superalloy
- Connecting the Microstructure Stability of Ni Based Superalloys to their Chemical Compositions
- Machining of Hastelloy-X Based on Finite Element Modelling
- Development of Multi-Objective Prediction Model for Wire Electrical Discharge Machining of Inconel 718 Nickel-Based Superalloy
- Prediction of Material Removal in Extrusion Honing of Hastelloy C22 Using Artificial Neural Network
- Modeling of the Structure of Heat-Insulating Semi-Transparent Materials and Coatings for Industrial and Transport Power Plants
- Microstructure Analysis and Creep Behaviour Modelling of Powder Metallurgy Superalloy
Les mer
Produktdetaljer
ISBN
9783035712636
Publisert
2020-08-21
Utgiver
Trans Tech Publications Ltd
Vekt
1020 gr
Høyde
240 mm
Bredde
170 mm
Dybde
27 mm
Aldersnivå
P, 06
Språk
Product language
Engelsk
Format
Product format
Heftet
Antall sider
530