The first issue of the topic series “Superalloys” contains articles published by Trans Tech Publications in 2017 year. The volume entitled as "Ni-Based Superalloys" provides the readers with a wide range of scientific research results and engineering solutions in the field of development, a study of properties and processing technologies of nickel-based superalloys. We hope this collection will be useful and interesting to a broad audience of researchers and engineers from the area of machinery.
Les mer
Aggregated Book
- Preface
- Chapter 1: Microstructure of Alloys
- The 3D Imaging and Metrology of Microstructural Elements in Innovative Materials for Clean Energy Systems and Aeronautics
- Metallography Evaluation of Cast and Wrought Ni-Base Superalloys
- Effect of Long-Term Aging on Microstructural Restoration in Cast Nickel Base Superalloy, GTD-111
- Effect of Temperature Dropping during Solution Treatment in Rejuvenation Heat Treatment and its Long-Term Heating Simulation on Microstructures of Nickel Base Alloy, Udimet 520
- Long-Term Gamma Prime Phase Stability after Various Heat Treatment Conditions with Temperature Dropping during Solution Treatment in Cast Nickel Base Superalloy, Grade Inconel-738
- Effect of Precipitation Aging Temperatures on Reheat Treated Microstructures and its Phase Stability after Long-Term Exposure in Cast Nickel Base Superalloy, Grade Inconel 738
- Effect of Solution Treatment Temperature on the Grain Growth Behavior of Fine Grained FGH96 Superalloy
- Effect of Strain Hardening on Precipitation Kinetics in ATI 718Plus
- Oxidation Behavior of a Disk Powder Metallurgy Superalloy
- Morphology Evolution of Grain Boundary Carbides in Highly Twinned Inconel Alloy 600
- Morphological Evolution of Carbides in DZ125 Superalloy during Heat Treatment
- Microstructure and Property Calculation of Three Typical Second Generation Single Crystal Superalloys
- The Precipitation Behavior of γ′ Phase in Single Crystal Ni-Based DD6 Superalloy for Turbine Blade
- A Review of Rafting in Nickel-Based Single Crystal Superalloys
- The Influence of γ/γ′ Morphology on the Rafting and Stress Distribution of Nickel-Based Superalloys Loaded in [0 0 1] Direction
- Chapter 2: Mechanical Behaviour and Deformation Modelling
- Small Ring Testing of High Temperature Materials
- Stabilities of Microstructure and Mechanical Properties during Long-Term Aging on FGH95 Superalloy
- Influence of Dynamic Strain Ageing and Long Term Ageing on Deformation and Fracture Behaviors of Alloy 617
- Influences of W and Al on the Microstructure and Stress-Rupture Property of Re-Free Ni-Based Single Crystal Superalloys
- Long Time High Temperature Stress Rupture Strength Behavior and Structure Stability Study on Ni-Base Superalloy Nimonic 80A
- Degradation of the Strength of Grains and Grain Boundaries of Ni-Base Superalloy under Creep and Creep-Fatigue Loadings
- Creep Processes in MAR-M247 Nickel-Base Superalloy
- Microstructure Evolution and Stress Rupture Properties of DD6 Single Crystal Superalloy after Overheating
- Microstructure Evolution and Creep Properties of a Single Crystal Nickel-Based Superalloy with Various Orientations
- High Temperature Rupture Life of Nickel-Based Superalloy under Directional Solidification with High Temperature Gradient
- Creep Behavior of a Ru-Free Nickel-Based Single Crystal Superalloy at Medium Temperatures
- Mechanical Behaviour of Materials during Creep with Changing Loads
- Interaction of Creep and High Cycle Fatigue of IN 713LC Superalloy
- Failure Assessment of the First Stage High Pressure Turbine Blades
- Fatigue Crack Initiation in Nickel-Based Superalloy MAR-M247 at High Temperature
- Effect of Maximum Temperature on the Thermal Fatigue Behavior of Superalloy GH536
- Characteristics of Microscopic Inclusions and their Influence on Fatigue Crack Propagation in FGH96 Superalloy
- Initiation and Propagation Behaviors of Small Crack in a Polycrystalline Ni-Base Superalloy under Thermo-Mechanical Fatigue Loading
- Effect of Frequency on the Fatigue Behavior of IN718 Superalloy
- Surface Roughness Effects on the Fatigue Behavior of As-Machined Inconel718
- Crystal Plasticity Simulations of Haynes 230, an Analysis of Single Crystal and Polycrystalline Experiments
- Fatigue Crack Propagation in Haynes 230: A Comparison between Single and Polycrystal Crack Closure Levels
- Fatigue Crack Growth in Flow Formed INCONEL 718
- Chapter 3: Solidification and Processing
- Effect of Hot Isostatic Pressing on Microstructures and Mechanical Properties of IN738LC Superalloy
- Effects of HIP Process on the Microstructure and Mechanical Properties of a Cast Superalloy
- Microstructure Study of Nickel-Based Superalloys after Deep Cold Rolling
- Analysis of Deformation and Internal Defect in Flat-Wedge Cross-Wedge Rolling of GH4169 Superalloy
- A Novel Unified Dislocation-Density Based Model for Hot Deformation Behavior of a Nickel-Based Superalloy
- Hot Deformation Behavior of AA-FGH720Li Superalloy
- The Addition of Zr in Nickel-Based Inconel 718 Superalloy to Prevent Hot Cracks Propagation
- Precision Casting of GTD222 Component with Complex Thin-Wall Structure
- Early Instability Phenomena of IN792 DS Superalloy
- Simulation and Experimental Studies on Grain Selection Behavior of DD5 Single Crystal Superalloy
- Microstructures of Low Angle Boundaries of a Third Generation Single Crystal Superalloy DD9
- The Effect of Process Parameters in Interdendritic-Melt Solidification Control Technique on the Microstructure and Properties of a Ni-Base Superalloy
- Effect of Low-Angle Boundary on Microstructure and Stress Rupture Property of a Third Generation Single Crystal Superalloy DD10
- Study on the Formation of Stray Grains during Directional Solidification of Nickel-Based Superalloys
- Chapter 4: Welding and Laser Deposition
- Thermal Cycle Simulation of Welding Process in INC 738 LC Superalloy
- Welding of IN792 DS Superalloy by High Energy Density Techniques
- IN792 DS Superalloy: Optimization of EB Welding and Post-Welding Heat Treatments
- The Microstructure of Inconel Alloys Used for Repair Welding
- Linear Friction Welding of IN718 to Ti6Al4V
- Measurement of Residual Stresses in Linear Friction Welded In-Service Inconel 718 Superalloy
- Investigation of Impact Behavior of TIG Welded Inconel 718 at Aircraft Engine Operating Temperatures
- Crack Growth Studies in a Welded Ni-Base Superalloy
- Evaluation on the Corrosion and Wear Resistance of Welding Zone Welded with Plasma Transferred Arc Welding Method
- Structure Formation in Ni Superalloys during High-Speed Direct Laser Deposition
- Preliminary Experimental Study of Laser Cladding Repair on Directionally Solidified Blades
- Effect of Build Orientation and Post Processing of a Direct Laser Deposited Nickel Superalloy as Determined by the Small Punch Creep Test
- A Study on the Microstructural Characterization of René 142 Deposited Atop René 125 Processed through Scanning Laser Epitaxy
- Brazing Inconel 600 Using the VZ-2150 Filler for Plate Heat Exchanger
- Brazing Inconel 600 to Manufacture the Plate Heat Exchanger
- Chapter 5: Thermal Barrier Coatings
- Phase Stability, Structure and Thermodynamics of Modified Ni- and Fe-Aluminides
- Durability of Amorphous and Crystalline BMAS Thermal Barrier Coatings Produced by Plasma Spraying
- Formation of Thermally Sprayed Coatings on Grid-Like Structure Substrate
- Research on the Stability of Thermal Barrier Coatings under Thermal Cyclic Loading
- Interdiffusion Databanks of γ, γ′ and β Phases in NiAl-Based Ternary Systems
- Cyclic Oxidation Performance of Si-Aluminide/MCrAlY Coating on Ni-Base GTD-111 Superalloy
- The Study of High Temperature Oxidation Performance of Thermal Barrier Coatings Prepared by Plasma Spraying and Laser Remelting
- Diffusion-Controlled Growth and Microstructural Evolution of Aluminide Coatings on Superalloys and Steel
- Sintering Study of NiCrAlY
- Effect of Double Electron Beam Remelting on Microstructure of HVOF and CGDS Bond Coat
- EBSD Analysis and Assessment of Porosity in Thermal Barrier Coatings Produced by Axial Suspension Plasma Spraying (ASPS)
- Development of the Advanced TBC for High Efficiency Gas Turbine
- Material and Mechanical Aspects of CMAS Damage Progression on Thermal Barrier Coatings and its Non-Destructive Detection
- Failure Mechanism of Yttria Stabilized Zirconia Atmospheric Plasma Sprayed Thermal Barrier Coatings Subjected to Calcia-Magnesia-Alumino-Silicate Environmental Attack
- Degradation of YSZ/EUCOR TBC Coating System during High Temperature Low Cycle Fatigue Tests
- The Application of the Small Punch Tensile Test to Evaluate the Ductile to Brittle Transition of a Thermally Sprayed CoNiCrAlY Coating
- Measurement of Young’s Modulus of Thermal Barrier Coatings by Suspended Coupled Flexural Resonance Method
- The High Temperature Creep Properties of a Thermally Sprayed CoNiCrAlY Coating via Small Punch Creep Testing
- Investigation on Fracture Toughness of Coating/Substrate Interface - Case Study: Thermally Sprayed Nickel Based Superalloy on Variety of Substrates
- Thermomechanical and Thermal Gradient Mechanical Fatigue Lifetime of Thermal Barrier Coating Systems
- Thermo-Mechanical and Low Cycle Fatigue Failure Behavior Relevant to Temperature Regime in a TBCed Superalloy Specimen
- Chapter 6: Machining Processes
- Specific Cutting Force in Turning of Sintered Nickel Alloy
- Manufacturing of Axisymmetric Components out of Superalloys and Hard-to-Deform Steels by Roll Forming
- Influence of Coolant Application Direction on the Cutting Performance of Ceramic Tool in High-Speed Air-Jet-Assisted Machining of Inconel 718
- Experimental Study on the Relationship of Discharge Parameters with Crack Arrest Effects in Inconel 625 Alloy by Electropulsing Treatment
- Machinability of Inconel 625 Aerospace Material Using Cryogenically Treated WEDM
- Experimental Study on Electro-Discharge Machining of Nickel-Based Superalloy
Les mer
Produktdetaljer
ISBN
9783035711615
Publisert
2020-07-28
Utgiver
Trans Tech Publications Ltd
Vekt
1340 gr
Høyde
240 mm
Bredde
170 mm
Dybde
36 mm
Aldersnivå
P, 06
Språk
Product language
Engelsk
Format
Product format
Heftet
Antall sider
720