17th International Symposium on Metallography, Fractography and Materials Science (April 24 – 26, 2019, Nový Smokovec, High Tatra Mountains, Slovak Republic). Collected articles focus on not only research in the field of steel, alloys, and metallic materials but also in the field of numerous modern materials and technologies - ceramics, composites, amorphous materials, special coatings, and powder metallurgy.

Les mer

Selected full text papers from the 17th International Symposium on Metallography, Fractography and Materials Science (2019)

Selected, peer-reviewed papers from the 17th International Symposium on Metallography, Fractography and Materials Science (Metallography XVII), April 24 – 26, 2019, Nový Smokovec, High Tatra Mountains, Slovak Republic

Les mer
  • Preface
  • Invited Lectures
  • Boronizing of AISI 316L Stainless Steel Using Spark Plasma Sintering Technique
  • Novel Cost-Efficient Method of Producing Ausferritic Steels Displaying Excellent Combination of Mechanical Properties
  • The Copper-Arsenic Eutectic and the Cu3As Phase
  • Metallographic Documentation of the Degradation of Iron and Nickel Based Alloys in HCl and H2S Containing Environments, between 480 – 680 °C
  • Characterisation of Chemical Vapour Deposited AlHfN Coatings
  • Chapter 1: Process Simulation and Metallographic Methods
  • The Influence of Surface Dipping and Bulk Filling Agents on Properties of High-Speed Grinding Wheels: Materialographic-Based Numerical Modelling
  • A Thermomechanical Model of Retention of a Diamond Particle in Matrices Based on Fe
  • Investigation of the Diffusion Couple Ductile Cast Iron / Iron
  • SEM Imaging of In Situ Tensile Testing of 27CrNiMoV Steel
  • Nanomechanical Characterization of Iron Borides in Fe-Mn-B Ternary Alloys
  • Chapter 2: Solidification and Solid State Transformation
  • Simultaneous Fabrication of Multiple Castings Using Frozen Mold Casting Method
  • The Effect of Heat-Treatment on the Phase Stability of Fe-28Al-15Si-2Mo Alloy
  • The Microstructure Evolution of Fe-28Al-15Si-0.2Zr Alloy during Different Heat-Treatment
  • Structural Nature of ZnAl4Cu1 Alloy Plasticity Affected by Various Technological Treatments
  • Microstructural and Fractographic Analysis of CuAlNi Shape Memory Alloy before and after Heat Treatment
  • Chapter 3: Interrelationship between Microstructure and Material Properties
  • Inclusion Engineering in Structural Steels with Enhanced Machinability
  • Texture Evolution during Cold Drawing of Steel Tube with Respect to the Stress - Strain State
  • Microstructure Influenced by Controlled Rolling, Cooling and Thermal Processing of Seamless Tubes Made of Steel 25CrMo4
  • Microstructure, Substructure and Mechanical Properties of 9CrNB Steel after Tempering
  • Comparison of Microstructure and Mechanical Properties of Additively Manufactured and Conventional Maraging Steel
  • Structure and Properties of Bakelite Bonded Grinding Wheels
  • The Influence of Secondary Phase on Impact Toughness of Alloyed Iron Aluminides
  • Biodegradable Iron-Based Foams for Potential Bone Replacement Material
  • Chapter 4: Welding
  • On the Surface Welding of Pearlitic Rails: The Control of Dilution and Microstructure
  • Analysis of the Cause of Damage to the Steam Generator Cold Collector’s Dissimilar Weld Joint at Slovak Nuclear Power Plant
  • Possibilities for Using New Types of Additive Materials for Hardfacing
  • Analysis of Causes of Baby Stroller Construction Damage
  • Chapter 5: Fractures, Defects and Material Degradation
  • Fractography of Additively Manufactured Titanium Alloy: Influence of Post-Processing Treatment
  • Influence of Boric Acid Solution and Gamma Irradiation on Selective Sorbents
  • Surface Chemistry-Based Surface Defects Situated on Steel Strips Edges
  • The Failure of Carbon Fiber Reinforced Composite Analyzed by Acoustic Emission
  • Size Effect in Plastic Deformation and Failure of Metallic Glasses
  • Analysis of Causes of Defects Appearance in Wire Drawing
  • Metallographic Analysis of Stainless Steel Inner Shaft of Centrifugal Pump
  • Investigation of Screw Failed During Installation
  • Rarely Occurring Defects on Tinplates
  • Defects of Steel Sheets Joined by Laser Welding
  • Analysis of Corrosion Resistance of Heat Exchanger Plates Made of AISI 316L Steel
  • Microstructural and Chemical Analysis of Military Steel from World War II as Part of Sculpture
  • Chapter 6: Fatigue and Creep
  • 3D Textural Analysis of Fatigue Fracture Surfaces
  • Character of Fatigue Damage under Axial, Torsional and Biaxial Loading of 316L Stainless Steel
  • The Effect of Prior Surface Roughness on Fatigue Life of Nitrided Specimens
  • Detection of Early Stage of Fatigue Changes in Non-Alloy Steel Using Residual Magnetic Field Method
  • Estimating of the Size of the Maximum Non-Metallic Inclusions in Martensitic Steels and their Influence on Fatigue Properties
  • The SEM and TEM Analysis of IN718 Alloy after Fatigue Push-Pull Loading at 700°C
  • Characterization of Microstructure of Crept Samples of Dissimilar Weld Joint Using Standard and Advanced Electron Microscopy Techniques
  • Evaluation of Cavitation Damage in a Pipe Bend Made of 0.5Cr-0.5Mo-0.3V Steel by Optical Metallography and Replica Method
  • Near-Surface Structure and Fatigue Crack Initiation Mechanisms of As-Built SLM Inconel 718
  • Fatigue Behavior of Titanium Endoprosthesis
  • Influence of Cyclic Loading on the Internal Friction Measured on Magnesium Alloys AZ31, AZ61 and AZ91
  • SnO2 Nano/Microfibers for Gas Sensors
  • Chapter 7: Nonferrous Alloys
  • Effects on Microstructure and Corrosion Behavior of a Heat Treated CuZn36Pb2 Brass
  • Small Scale Plastic Yielding of Mg Alloys Assessed with Nanoindentation
  • Magnesium Alloy WE43 Produced by 3D Printing (SLM)
  • Experimental Verification of Phase Diagram Calculations of Zr-Based Alloys after High-Temperature Oxidation
  • Consequences of Inappropriate Temperatures of the Solution Heat Treatment in Al-Si-Cu Cast Alloys
  • Characterization of High-Speed Alumina Abrasive Grinding Wheel
  • Chapter 8: Powder Metallurgy
  • Step-Sintering of Fe-(1-3)%Mn-0.8%C Steels
  • Microstructure and Mechanical Properties of Fe-Cu-Ni Sinters Prepared by Ball Milling and Hot Pressing
  • Characterization of Mg-Zn Layered Bulk Materials Prepared by Powder Metallurgy Method
  • Influence of Oxide Dispersoids on the Structure Development of Copper Nanocomposite Prepared by Spark Plasma Sintering Technology
  • Preparation of Cerium Stabilized Zirconia Bulk Ceramics by Spark Plasma Sintering
  • Sintering of High Mn Cemented Carbides in Mn-Rich Environment
  • Chapter 9: Surface Engineering and Coatings
  • Microstructure, Stiffness and Corrosion of Bare and Phosphated Specimens Made by Sintering of Structured Iron-Iron Oxide Spheres
  • Thermal Cyclic Behaviour of Conventional YSZ and Mullite-YSZ Thermal Barrier Coatings
  • Influence of RF Plasma Jet Surface Treatment on Wetting Behavior of Yttria Stabilized Zirconia SPS Coatings
  • Microstructure Characteristics, Tribology and Nano-Hardness of Plasma Sprayed NiCrRe Coating
  • Microstructure Characteristics, Tribology and Nano-Hardness of HVOF Sprayed NiCrRe Coating
  • Anodizing of Pure Magnesium in Sodium Hydroxide Electrolyte Solution
Les mer

Produktdetaljer

ISBN
9783035716122
Publisert
2020-12-16
Utgiver
Trans Tech Publications Ltd
Vekt
930 gr
Høyde
240 mm
Bredde
170 mm
Dybde
24 mm
Aldersnivå
P, 06
Språk
Product language
Engelsk
Format
Product format
Heftet
Antall sider
470